OEM/ODM Manufacturer 316L Chemical Injection Line - Monel 400 Capillary Tube Chemical Injection Line – MEILONG

Short Description:


Product Detail

Product Tags

Related Video

Feedback (2)

Bear "Customer first, Excellent first" in mind, we operate closely with our customers and supply them with efficient and expert services for Alloy 625 Chemical Injection Line Tube, S32750 Control Line Tubing, Incoloy 825 Capillary Tube Control Line, As an expert specialized within this field, we've been committed to solving any problem of high temperature protection for users.
OEM/ODM Manufacturer 316L Chemical Injection Line - Monel 400 Capillary Tube Chemical Injection Line – MEILONG Detail:

Testing Abilities

Chemical Flare Metallurgical
Corrosion Flatten Positive material identification (PMI)
Dimensional Grain size Surface roughness
Eddy current Hardness Tensile
Elongation Hydrostatic Yield

Application

In all fields of the oil and gas industry, chemicals are injected into process lines and fluids. Take oilfield services, chemicals are used to film the side of the wellbore for improved stability. In pipelines they avoid build-up and keep the infrastructure healthy.

Other Application:

In the oil and gas industry we inject chemicals in order.
To protect the infrastructure.
To optimize processes.
To assure flow.
And to improve productivity.

Product Display

Monel 400 Capillary Tube Chemical Injection Line (3)
Monel 400 Capillary Tube Chemical Injection Line (1)

Alloy Feature

Characteristics

Corrosion resistance in an extensive range of marine and chemical environments. From pure water to non-oxidizing mineral acids, salts and alkalis.
This alloy is more resistant to nickel under reducing conditions and more resistant than copper under oxidizing conditions, it does show however better resistance to reducing media than oxidizing.
Good mechanical properties from subzero temperatures up to about 480C.
Good resistance to sulfuric and hydrofluoric acids. Aeration however will result in increased corrosion rates. May be used to handle hydrochloric acid, but the presence of oxidizing salts will greatly accelerate corrosive attack.
Resistance to neutral, alkaline and acid salts is shown, but poor resistance is found with oxidizing acid salts such as ferric chloride.
Excellent resistance to chloride ion stress corrosion cracking.

Chemical Composition

Nickel

Copper

Iron

Manganese

Carbon

Silicon

Sulfur

%

%

%

%

%

%

%

min.

 

max.

max.

max.

max.

max.

63.0

28.0-34.0

2.5

2.0

0.3

0.5

0.024


Product detail pictures:

OEM/ODM Manufacturer 316L Chemical Injection Line - Monel 400 Capillary Tube Chemical Injection Line – MEILONG detail pictures


Related Product Guide:

While using the "Client-Oriented" organization philosophy, a rigorous top quality command process, highly developed production devices and a potent R&D workforce, we normally provide high quality products, outstanding solutions and aggressive charges for OEM/ODM Manufacturer 316L Chemical Injection Line - Monel 400 Capillary Tube Chemical Injection Line – MEILONG , The product will supply to all over the world, such as: Holland, Latvia, Jamaica, We set "be a creditable practitioner to achieve the continuous development and innovation" as our motto. We would like to share our experience with friends at home and abroad, as a way to create a bigger cake with our joint efforts. We have several experienced R & D persons and we welcome OEM orders.
  • This supplier's raw material quality is stable and reliable, has always been in accordance with the requirements of our company to provide the goods that quality meet our requirements.
    5 Stars By Catherine from Croatia - 2017.05.21 12:31
    The supplier abide the theory of "quality the basic, trust the first and management the advanced" so that they can ensure a reliable product quality and stable customers.
    5 Stars By Claire from Slovakia - 2017.12.19 11:10
    Write your message here and send it to us